Prints not sticking to the bed: first-layer and warping fixes for FDM printers
If a print will not stick to the bed, check four things first: a build plate free of skin oils, the right plate type and bed temperature in the slicer, the nozzle height on the first layer, and cold drafts around the print. Manufacturers publish different figures, so follow the documentation for your own printer and build plate before anything else.
Why a print does not stick to the bed
Manufacturers list broadly the same causes. Bambu Lab names skin oils from fingerprints as the top cause; the rest come down to settings, the machine and the room.
- A dirty build plate: fingerprints, grease, dust or old glue residue. This is on the cause lists from Bambu Lab, Prusa, Anycubic and Elegoo.
- The plate type chosen in the slicer does not match the plate on the printer. Bambu Lab’s example: slicing for the Cool Plate (PLA at 35°C) but printing on Textured PEI, which needs 55–65°C, leaves the bed far too cold. On Textured PEI the printer also lowers the nozzle by 0.04 mm after bed levelling, so the wrong plate type leaves the nozzle too high.
- The nozzle is too far from the bed on the first layer, i.e. the Z offset is too high, according to Bambu Lab. Prusa also lists wrong nozzle height as a cause.
- Bed temperature, nozzle temperature or speed that does not suit the material (Prusa). Anycubic adds first-layer flow that is too low, first-layer speed that is too high, and a first-layer fan that is too strong.
- Bed levelling that did not finish or is inaccurate. Bambu Lab says levelling data from an earlier calibration can occasionally be inaccurate; Elegoo mentions a tilted heated bed, abnormal levelling data and a build plate that is not seated properly.
- Damp filament. Bambu Lab says to listen for crackling or popping and look for a rough, bubbly surface, and to dry the filament before trying again. Prusa also lists a full or partial clog, and Anycubic a slightly clogged or worn nozzle.
- Cold air on the print. Bambu Lab says a nearby open window, air-conditioning vent or desk fan can cool one side of a print faster than the other, and that in a room below 20°C warping can occur even with PLA and PETG.
- Too small a contact area between the model and the plate (Anycubic).
- A worn plate. Prusa says a PEI surface can lose its adhesion after a couple of hundred hours of use.
Clean the build plate the way its maker says
Cleaning advice differs between manufacturers and some of it points in opposite directions: Bambu Lab prefers dish detergent to alcohol on Textured PEI, while Prusa has you wipe with IPA before every print. Check whose plate you have and follow that plate’s instructions.
- Bambu Lab Textured PEI: wet the plate, apply dishwashing detergent, scrub with a sponge or plastic brush, rinse with warm water and dry with a paper towel. The detergent must not contain oils or moisturisers. Hold the plate by its sides, and do not touch the print surface with bare hands after cleaning.
- Bambu Lab’s reason for detergent rather than alcohol on Textured PEI: alcohol might just spread the oils over the print surface instead of removing them.
- Bambu Lab’s water test: if water forms a thin film, the plate is clean; if it runs in streams and beads up, adhesion will be poor.
- Bambu Lab says not to clean Textured PEI with acetone because it damages the PEI surface, and its filament guide also warns against cleaning the plate with acetone.
- Bambu Lab Cool Plate SuperTack: clean with dish soap and water; no stiff-bristled brush and no acetone. The same page is inconsistent about alcohol: one passage rules out isopropyl alcohol, another allows a gentle wipe with alcohol.
- Prusa: wipe the print surface with isopropyl alcohol (IPA) of 90% or stronger before every print. Its stated reason is that lower concentrations may contain unsuitable additives.
- If adhesion drops over time, Prusa says to wash with warm (not hot) water and a few drops of dish soap, not to soak the sheet, and to dry it well.
- Prusa allows acetone only on the smooth PEI sheet and only occasionally; never on textured or satin sheets, and not before printing PETG.
- Anycubic Kobra X: clean with isopropyl alcohol and a lint-free cloth. Do not use wet wipes, make sure glue and grease are fully removed and the surface is completely dry, and do not touch the plate afterwards.
- Elegoo Centauri Carbon 2 Combo: clean dust, oil and filament residue off the build plate. The FAQ names no cleaning agent.
Bed temperatures, manufacturer by manufacturer
The figures below are each manufacturer’s own, as published. They cannot be averaged or swapped between brands; start from the line that matches your printer, build plate and filament brand.
If the first layer still grips weakly, Bambu Lab and Anycubic (Kobra X) say to raise the bed by 5–10°C, and Prusa says 5–10°C for difficult materials. Hotter is not always better: Polymaker lists excessive bed heat, for example PETG above 80°C, as a cause of over-adhesion.
- Bambu Lab (filament guide table, by plate): PLA 35–45°C on the Cool Plate and 45–65°C on the Engineering Plate (glue required), Smooth PEI and Textured PEI; PETG 60–80°C; ABS and ASA 90–100°C. The Cool Plate is not recommended for PETG, ABS or ASA.
- Bambu Lab’s figures vary by page: PLA on Textured PEI is 45–65°C in the table, while its warping page gives a target of 55–65°C. For the Cool Plate the table gives 35–45°C, while the warping page uses 35°C in its example.
- Bambu Lab Cool Plate SuperTack: PLA adheres firmly at a 40°C bed. On the second-generation plate PETG needs 55–60°C, though some printers (X and P series) may still use about 65°C.
- Prusa (filament material table): PLA 50–60°C, PETG 70–90°C, ABS 95–110°C, ASA 90–110°C. Prusa’s individual material pages may give different figures from this table, so open the page for your material as well.
- Polymaker: PLA 40–65°C as a general range (50–60°C for Polymaker’s own PLA). PETG is 60–80°C on one page and 65–90°C on another; ABS is 80–110°C on one page and 100–110°C on another.
- Anycubic Kobra X starting points: PLA 50–65°C, PETG 70–85°C, ABS 90–110°C, TPU 45–60°C.
- Elegoo Centauri Carbon 2 Combo: the FAQ has no per-material table and says to use ELEGOO’s official parameters or the filament manufacturer’s recommended settings. The heated bed reaches a maximum of 110°C.
- On enclosed Bambu Lab printers, with the bed above 45°C for PLA, TPU or PVA, or above 60–70°C for PETG, Bambu Lab recommends opening the front door or removing the top glass cover so the filament does not soften in the extruder. This does not apply to ABS, ASA, PC or PA.
- Polymaker warns that a printer’s internal sensors may misread by 5–10°C, and that uneven bed heating is common on larger printers.
When to use glue, and on which plate
In the manufacturers’ documentation glue does two jobs: it helps stubborn materials stick, and it acts as a barrier so a print does not bond hard enough to damage the plate on removal. Whether to use it depends on the plate and the material.
- Bambu Lab says a standard glue stick applied in a thin, even layer dramatically improves adhesion for stubborn filaments, especially ABS, ASA, PA and PC. Thick blobs cause an uneven first layer. The glue dissolves in water.
- Bambu Lab Smooth PEI: only PLA goes without glue; other filaments need it to stop the PEI sheet tearing.
- Bambu Lab Textured PEI: PC, PA, ABS or ASA may need a layer of glue stick.
- Bambu Lab Engineering Plate: the filament table requires glue for PLA.
- Prusa: use a basic PVA-based glue stick. It is not needed for PLA but is advisable for nylon, PETG, PC, PET-based materials, ABS, ASA and flexible materials. Enable a brim before reaching for adhesives, apply the glue thinly to the cold sheet, and never put superglue on the sheet.
- Polymaker recommends a glue stick for PETG on smooth PEI, and says glass or smooth plates often require an adhesive for PLA.
- Anycubic Kobra X: for some materials, a thin layer of an approved adhesion aid on the build plate can improve first-layer grip.
First-layer settings: nozzle height, speed and fan
Once the plate is clean and the bed temperature is right, what remains is the first-layer setup. Anycubic warns against changing first-layer settings at random.
- Nozzle height: Bambu Lab says a Z offset that is too high leaves the nozzle too far from the bed on the first layer. Prusa says to lower Live Adjust Z slightly to increase adhesion, but not to over-squish the first layer; on the MK2 to MK3.5 a nozzle that is too close blocks extrusion.
- Bed levelling: Bambu Lab says to keep Bed Leveling Calibration turned on when starting a print. Anycubic Kobra X says to re-run auto-leveling. Elegoo says that if part of the first layer is too thin or too thick, clean the plate, make sure it is installed flat and run auto-leveling again.
- Speed: Prusa says to lower print speed to about 75% for the first three layers and then return to normal. Elegoo also says to reduce first-layer speed.
- Fan: Bambu Lab says most common filaments should have no cooling for the first 3 layers (set “No cooling for first X layers” to 3). Anycubic Kobra X says to keep the fan low or off for the first layer; Elegoo says to turn it off or down for the first few layers.
- Preheating: Polymaker says to preheat the bed for 10–15 minutes so the temperature is uniform across the plate.
Warping and lifting corners
Bambu Lab explains warping as thermal shrinkage: the outer edges of a print cool faster than the centre. It is more common with larger prints, higher infill density and ABS, ASA, PC, PA and PA-CF, and Bambu Lab ranks the risk from high to low as PC, PA-CF, PA, ABS, ASA, PETG, PLA. For large flat prints it suggests PLA, PLA-CF, PETG or PETG-CF.
On ABS the manufacturers do not write the same thing. Bambu Lab’s ABS advice is a hotter bed and a closed, warm chamber, with a brim among its quick fixes for warping in general. Prusa lists a brim as one of several warping fixes. Elegoo recommends a brim for materials that shrink easily. Polymaker writes about the enclosure. Check which approach your own printer’s documentation gives.
- Bambu Lab’s three quick fixes: clean the plate with soap and water, raise the bed temperature by 5–10°C, and add a brim or brim ears.
- PLA corners lifting (Bambu Lab): raise the bed by 5–10°C, aim for 55–65°C on Textured PEI, and add a brim 8–10 mm wide.
- ABS or ASA corners lifting (Bambu Lab): raise the bed by 10–15°C and close all doors and the top cover; the chamber should reach 40°C or more. On an open-frame printer such as the A1 with a warp-prone filament, raise the bed by 10°C.
- Bambu Lab says ABS, ASA, PA and PC need an enclosed printer with a heated chamber, and that large flat ABS, ASA or PC prints will almost always warp without an enclosure.
- Large flat models (Bambu Lab): use Gyroid infill at 25% or less, because Grid and Triangle patterns create internal linear tension.
- Bambu Lab brim ears: set the brim type to Painted and use the Brim Ears tool on the lifting corners only.
- Prusa: stabilise the ambient temperature or use an enclosure, use the skirt as a draft shield, orient problem areas toward the centre of the bed, decrease print speed, add a brim and apply a thin layer of glue stick. It also warns that printing PLA or PETG in an enclosure might not be a good idea, since both need strong cooling.
- Elegoo: increase the heated bed temperature, reduce first-layer speed, turn off or reduce the fan for the first few layers, and keep cold air from blowing directly onto the print area. For materials that shrink easily, use a brim or a more suitable printing environment.
- Anycubic Kobra X: reorient the model so the first layer has a larger contact area, and use a brim when the base is small.
- Polymaker describes an enclosure as mandatory for temperature stability with ABS and required for warping prevention with ASA.
Before you remove the part: plate-care warnings
A print that sticks too hard can damage the plate as well. These warnings come from each manufacturer’s own documentation.
- Bambu Lab says to wait for the plate to cool before removing a part: 35°C or lower on Textured PEI. Then bend the plate to release it, which avoids scratching the plate or damaging the bottom of the model.
- Bambu Lab Cool Plate SuperTack is designed only for PLA and PETG; other materials may damage the surface coating.
- Prusa warns that PETG and PC can adhere strongly enough to damage the PEI surface.
- Elegoo warns that after printing ABS, ASA or PC you should not touch the nozzle, heated bed or bottom of the model immediately, to avoid burns, and should pay attention to ventilation.
Pertanyaan yang sering diajukan
Does PLA need glue to stick?
It depends on the plate. Bambu Lab says PLA needs no glue on Smooth PEI but does on the Engineering Plate. Prusa says a glue stick is not needed for PLA, and Polymaker says glass or smooth plates often require an adhesive. Clean the plate and check the bed temperature in your plate’s documentation first.
Can I wipe the build plate with alcohol?
It depends on the manufacturer. Prusa says to use IPA of 90% or stronger before every print, and Anycubic Kobra X says isopropyl alcohol with a lint-free cloth. Bambu Lab has you wash Textured PEI with dish detergent instead, because alcohol might just spread the oils over the plate.
Can I clean the plate with acetone?
Bambu Lab says not to clean its plates with acetone and that it damages the Textured PEI surface. Prusa allows it only on the smooth PEI sheet, occasionally, never on textured or satin sheets, and not before printing PETG. If you are not sure which plate you have, hold off.
My ABS corners lift every time. What should I do?
Bambu Lab says to raise the bed by 10–15°C and close the doors and top cover so the chamber reaches 40°C or more, and that large flat ABS prints will almost always warp without an enclosure. Polymaker also describes an enclosure as mandatory for ABS. A thin layer of glue stick improves ABS adhesion according to Bambu Lab.
Does air conditioning or a fan in the room affect the print?
Yes. Bambu Lab says a nearby air-conditioning vent, open window or desk fan can cool one side of a print faster than the other, and that below 20°C warping can occur even with PLA and PETG. Prusa suggests using the skirt as a draft shield, and Polymaker says to add 5–10°C to the bed for PLA in a cold room.
Why does the first layer stick in some areas but not others?
Elegoo lists build plate contamination, a tilted heated bed, abnormal levelling data or a plate that is not installed properly: clean the plate, make sure it sits flat and run auto-leveling again. Prusa adds a bent sheet or debris under the sheet. Polymaker says uneven bed heating is common on larger printers and recommends preheating the bed for 10–15 minutes.
Manufacturer sources
- Bambu Lab Wiki — First Layer Not Sticking: Causes and Solutions
- Bambu Lab Wiki — Model Warping, Falling Off, or Collapsing
- Bambu Lab Wiki — Bambu Lab Textured PEI Plate Cleaning Guide
- Bambu Lab Wiki — Filament guide: Printer, Nozzle, AMS, Build Plate, Glue Compatibility
- Bambu Lab Wiki — Introduction to Bambu Lab Build Plates
- Prusa Knowledge Base — First layer issues
- Prusa Knowledge Base — Warping
- Prusa Knowledge Base — Prusa Filament Material Guide
- Polymaker Wiki — Build Plate Temperature
- Polymaker Wiki — By Material Type
- Anycubic Wiki — Kobra X: Model Non-stick HotBed Troubleshooting
- ELEGOO Wiki — Centauri Carbon 2 Combo FAQ