Print My Design

Washing and UV-curing resin prints: the order, the times and the safety rules

Ditulis oleh tim Print My Design · diperbarui 2026-11-26

To wash and UV-cure a resin print, put on nitrile gloves, wash off the uncured resin in the liquid your resin maker specifies, let the part dry completely, then post-cure it under UV light. IPA strength, wash time and cure time differ widely between manufacturers: Phrozen limits its RPG resin to 60 seconds in alcohol, while the Prusa CW1 defaults to a 3-minute wash. Follow the instructions for your own resin first.

The wash and UV-cure sequence, in order

A print fresh off the machine still carries uncured resin on its surface. The manufacturer guides we collected all put the main steps in the same order: wash, dry, then UV-cure.

The numbers inside each step are not the same. Elegoo says in its Wiki that washing and post-curing time depend on the resin type, the size and structure of the model, and the equipment, and that you should follow the recommended settings for that resin and that washing and curing equipment.

What to wash with, and how strong the IPA should be

The wash liquid depends on the resin. Elegoo says in its Wiki that standard resin is generally cleaned with isopropyl alcohol (IPA) or ethyl alcohol at the concentration the resin manufacturer specifies, or with a compatible specialised cleaning solution. Water-washable resin should be cleaned with water or another specified medium, and one cleaning method should not be applied arbitrarily to different resin types.

Anycubic's store article is explicit that only models printed in water-washable resin can be washed with water.

The concentration figures differ by manufacturer. We list them side by side and do not average them.

How long to wash, and what over-soaking does

Wash time is where the figures differ most: from dips of no more than 20 seconds to soaks of 10–12 minutes, depending on the resin formula and the liquid. Use the figure for the resin you actually have, not another brand's.

Soaking too long does damage. Prusa does not recommend washing in IPA for more than 10 minutes, because tiny cracks may appear, sometimes more than 24 hours later. Anycubic's store article explains that over-soaked parts absorb too much liquid and swell, then crack or turn brittle.

Manufacturers do not agree on ultrasonic cleaners. Siraya Tech and Phrozen include the method in their guides, but Anycubic's store article warns that in an ultrasonic cleaner filled with IPA the high-frequency vibrations can create sparks and start a fire. Read both the resin guide and the cleaner's manual before using one.

Dry the part completely before UV curing

Do not cure a wet part. Elegoo warns that white impurities may appear if the model is not completely dry, and Anycubic's Wiki lists curing immediately after washing as one cause of white parts and says to air-dry first.

For hollow models, drain any remaining liquid and dry both the surface and the interior. Elegoo says this reduces the risk of later cracking or deformation.

How long to UV-cure, and at what wavelength

Manufacturer cure times run from 1–2 minutes to 30 minutes. Elegoo says curing time varies with model size and structure; its Wiki gives no fixed number and tells you to follow the recommended settings for the resin.

On wavelength, Elegoo says to use a 405 nm UV lamp, the same wavelength as its printers. Siraya Tech specifies 395–405 nm and warns in the Magna Durable manual that light sources below 395 nm make the model yellow quickly.

Curing for too long also does harm. Elegoo says both insufficient and excessive post-curing may reduce model performance, and that excessive post-curing may accelerate yellowing in some materials.

Remove supports before or after UV curing?

There is no single answer here, because the manufacturer guides differ. If the guide for your resin names a stage, follow that first.

Safety, and disposing of wash liquid and resin waste

Protective equipment as the manufacturers list it: Elegoo names nitrile gloves, a protective mask, safety goggles and an apron, and says to protect your eyes during curing. Siraya Tech names nitrile gloves, safety glasses and a respirator rated for organic vapours. Prusa says to always wear protective gloves when handling resin, recommends a simple respirator, and says to keep the room ventilated during printing because resin produces fumes.

IPA and alcohol are flammable. Prusa calls isopropyl alcohol a volatile flammable liquid. Anycubic's store article calls a manual bath dangerous because the IPA is in the open air. Phrozen says to store used liquid in an airtight container.

On disposal, manufacturers treat liquid waste and cured solids separately, and their wording is not identical. We quote each as written. Your local waste disposal rules decide how you actually dispose of it.

Pertanyaan yang sering diajukan

My print is still sticky after curing. What should I do?

The advice depends on the cause. Elegoo says to continue cleaning until the surface stays dry and non-sticky. Prusa says to run the cure again if the part is still sticky. Anycubic's store article says that if the wash was incomplete, give the part two baths with fresh IPA and a soft brush.

Why did my print turn white after washing and curing?

Anycubic's Wiki puts it down to alcohol below 95% or curing straight after washing without drying. Elegoo lists wider causes: insufficient cleaning, residual cleaning solution, incomplete drying, abnormal curing conditions or the material itself, and notes that whitening alone does not necessarily indicate insufficient curing. Elegoo's fix is to clean again with fresh solution, dry the part fully and check the exposure.

Why did my print crack days later?

Manufacturers point to two groups of causes. One is soaking too long: Prusa does not recommend more than 10 minutes in IPA because tiny cracks may appear more than 24 hours later. The other is resin or cleaning solution trapped inside a hollow model: Elegoo says to add drainage holes, drain the liquid, dry the inside and outside before post-curing, and store the part somewhere cool, dry and away from the sun.

Can I pour the wash water from water-washable resin down the drain?

No. Elegoo says wastewater from water-washable resin must be collected and disposed of properly, and that filtering or curing the waste liquid does not mean it can be discharged directly into the sewage system. Follow the waste disposal rules where you live.

Does a longer UV cure make the part stronger?

Not necessarily. Elegoo says both insufficient and excessive post-curing may reduce model performance, and that excessive post-curing may accelerate yellowing in some materials. Siraya Tech warns in the Magna Durable manual that light sources below 395 nm make the model yellow quickly. Use the time your resin maker gives.

What should I do if resin gets on my skin?

Wash it off immediately with soap and water; Prusa and Siraya Tech both say so. Siraya Tech adds that you should not use solvents on skin. Prusa says to seek medical assistance for itching or eye contact. Elegoo says to follow the first-aid measures in the resin's safety data sheet (SDS) and to seek medical attention for discomfort, eye contact or swallowing.

Manufacturer sources

Lanjutkan di toko

Resin for 3D printersParts & accessoriesPrinter 3DFilamen & resin

Panduan lainnya

Model 3D gratis: tempat mengunduh dan cara mencetaknyaPerangkat lunak desain 3D untuk pencetakan 3D: mana yang harus dipilihPemindaian 3D: apa itu, untuk apa, dan cara memilih pemindaiBiaya pencetakan 3D: apa yang mendorong harga dan cara menguranginyaWet filament: how to spot it, dry it and keep it dryPrints not sticking to the bed: first-layer and warping fixes for FDM printers